Ke hoʻohālikelike ʻia me nā pōhaku lepo alumina maʻamau, loaʻa i kā mākou mau ʻāpana alumina māmā māmā nā hiʻohiʻona penei:
Haʻahaʻa puʻupuʻu nui. Ke hoʻohālikelike ʻia me nā pōhaku lepo alumina maʻamau me 99% AI2O3 maʻiʻo a me ka nui o ka nui o ka liʻiliʻi o 1.5 g/cm3, hiki i ka ultra-lightweight alumina bubble bricks ke hoʻemi i ke kaumaha o ke kino umu e mālama pono i nā mea waiwai, ikehu a me nā kumukūʻai;
ʻOi aku ka maikaʻi o ke kūpaʻa haʻalulu wela i hoʻohālikelike ʻia me nā pōhaku lepo alumina maʻamau me ka nui o 1.5 g/cm3 a me AI2O3≥99%;
ʻO ka haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa, ʻo 30% wale nō o nā huahana kuʻuna, Ma 400 ℃, ʻo ka conductivity wela o ka ʻili wela o ka alumina bubble brick me ka nui o 1.5g/cm3 a me AI2O3≥ 99% he 0.78w/(mK), ʻoiai ka thermal conductivity o ka umu wela aoao o Rongsheng's
ʻO 0.26w/(mK) nā pōhaku lepo alumina ultra-māmā, a ʻo kona hopena insulation thermal he 3 mau manawa o ka mea maʻamau. ʻO ka hoʻohana ʻana i nā pōhaku lepo alumina ultra-māmā e hiki ke hoʻohaʻahaʻa i nā ʻaoʻao anuanu ma lalo o ke koi like o ka mānoanoa o ka papa insulation a ʻoi aku ka nui.
mālama ikehu, a thinner insulation papa ma lalo o ka like koi o ke anuanu aoao wela.
Hiki ke hoʻohana pololei i ka papa hana o ka umu, a he ikaika ke kū'ē i ka erosion o ka hydrogen fluoride i loko o ka umu no ka mea anode.
ʻO ka hoʻomanawanui nui i loko o 0.05mm, hiki ke hoʻololi ʻia nā ana e like me nā koi o ka mea kūʻai aku.
Hōʻike
'ikamu | RS-KXQ1 |
BD,(g/cm3) | ≤0.85 |
CCS,(MPa) | ≥3 |
TC,400 ℃(W/m ·K) | ≤0.26 |
PLC (1500℃*6),% | ≤1.0 |
Al2O3, % | ≥99% |